Material Notes:
TLS H13 tool steel is a versatile chromium-molybdenum hot work steel that is widely used in hot work and cold work tooling applications. The hot hardness (hot strength) of H13 resists thermal fatigue cracking which occurs as a result of cyclic heating and cooling cycles in hot work tooling applications. Because of its excellent combination of high toughness and resistance to thermal fatigue cracking (also known as heat checking) H13 is used for more hot work tooling applications than any other tool steel. Because of its high toughness and very good stability in heat treatment, H13 is also used in a variety of cold work tooling applications. In these applications, H13 provides better hardenability (through hardening in large section thicknesses) and better wear resistance than common alloy steels such as 4140. Typical applications include inserts, cores, and cavities for die casting dies, die casting shot sleeves, hot forging dies, extrusion dies, and plastic mold cavities and components that require high toughnessTimken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.75 g/cc
7.75 g/cc
Density 7.75 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 50
50
Air Cooled from 982°C, 30 minutes
52.5
52.5
Air Cooled from 1010°C, 30 minutes
54
54
Air Cooled from 1032°C, 30 minutes
Modulus of Elasticity 207 GPa
30000 ksi
159 GPa

@Temperature 538 °C
23000 ksi

@Temperature 1000 °F
186 GPa

@Temperature 204 °C
27000 ksi

@Temperature 400 °F
Machinability 65 - 70 %
65 - 70 %
1% Carbon Steel
Charpy Impact 8.13 J
6.00 ft-lb
V-Notch; Air Cooled from 1010°C; 535°C Temper Temperature
19.0 J
14.0 ft-lb
V-Notch; Air Cooled from 1010°C; 635°C Temper Temperature
35.3 J
26.0 ft-lb
V-Notch; Air Cooled from 1010°C; 260°C Temper Temperature
Thermal Properties Metric English Comments
CTE, linear 11.3 µm/m-°C

@Temperature 21.0 - 204 °C
6.28 µin/in-°F

@Temperature 69.8 - 399 °F
13.5 µm/m-°C

@Temperature 21.0 - 538 °C
7.50 µin/in-°F

@Temperature 69.8 - 1000 °F
Thermal Conductivity 17.6 W/m-K

@Temperature 27.0 °C
122 BTU-in/hr-ft²-°F

@Temperature 80.6 °F
23.4 W/m-K

@Temperature 204 °C
162 BTU-in/hr-ft²-°F

@Temperature 399 °F
26.8 W/m-K

@Temperature 649 °C
186 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Component Elements Properties Metric English Comments
Carbon, C 0.40 %
0.40 %
Chromium, Cr 5.25 %
5.25 %
Iron, Fe 90.6 %
90.6 %
Manganese, Mn 0.40 %
0.40 %
Molybdenum, Mo 1.35 %
1.35 %
Silicon, Si 1.0 %
1.0 %
Vanadium, V 1.0 %
1.0 %
Chemical Properties Metric English Comments
Critical Temperature 802 °C
1480 °F
Ar1
826 °C
1520 °F
Ar3
840 °C
1540 °F
Ac1
890 °C
1630 °F
Ac3
Users viewing this material also viewed the following: