Loctite® 571 Thread Sealant

Category Polymer , Adhesive , Thermoset
Manufacturer Loctite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 571 Thread Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high pressure applications, liquid thread sealants seal instantly for low pressure testing. When fully cured, they seal to the burst strength of most piping systems.Loctite® Pre-Applied Thread Sealants are dry-to-the-touch films applied to threaded fittings by fitting suppliers and process centers located throughout North America. Pre-applied thread sealants are ideal for OEMs because they can improve speed of assembly and ensure quality by eliminating on-line dispensing of sealants.Loctite® 571 Thread SealantSeals operating pressures to 10,000 psi. Recommended Primer: 7649 (N)Typical Use: Excellent Solvent Resistance
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Viscosity 20000 cP
20000 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F