Lubrizol Advanced Materials PEARLCOAT® DIPP-119 Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlcoat®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLCOAT® DIPP-119 Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEARLCOAT® DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this product offers excellent flexibility, elasticity and easy processing. PEARLCOAT® DIPP-119 is used mostly in extrusion applications where low melting point as well as improved adhesion over polar substrates is highly appreciated. It is ideal for PVC compounding. It is also used in solvent coatings on textile substrates.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength, Yield 20.04 MPa
2906 psi
ASTM D412
Elongation at Break 750 %
750 %
ASTM D412
100% Modulus 0.00300 GPa
0.435 ksi
ASTM D412
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D412
Tear Strength 50.1 kN/m
286 pli
ASTM D624 (Die C)
Abrasion 45
45
loss (mm³); DIN 53.516
Thermal Properties Metric English Comments
Melting Point 118 - 128 °C
244 - 262 °F
MQSA 111
Glass Transition Temp, Tg -30.0 °C
-22.0 °F
DSC, 10ºC/min; DIN 51.007
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
MQSA 44