Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 300% Modulus = 0.580 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00400 GPa
0.580 ksi
ISO/R527
Polykemi AB POLYelast TPE Z700 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
300% Modulus 0.00400 GPa
0.580 ksi
ISO/R527
Polykemi AB POLYelast TPE Z706 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
300% Modulus 0.00400 GPa
0.580 ksi
ISO/R527
Polykemi AB POLYelast TPE Z706EX Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D412
Polimeri Europa Europrene® SOL TH 2314 Styrene - Ethylene / Butylene Block Copolymer
Europrene® SOL TH 2314 is a linear block copolymer obtained by selective hydrogenation of styrene-butadiene-styrene block copolymers. The polymer is based on styrene and ethylene/butylene, where b..
300% Modulus 0.00400 GPa
0.580 ksi
ISO/R527
Polykemi AB POLYelast TPE ZSB60650 Thermoplastic Elastomer, SEBS/SBS-based, Mineral Reinforced
Information provided by Polykemi AB
300% Modulus 0.00400 GPa
0.580 ksi
Injection molded parts; DIN 53504
Huntsman IROGRAN® CA116-203 TPU-Polyester
Introduction: IROGRAN CA116-203 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-203 is part of the HUNTSMAN film and shee..
300% Modulus 0.00400 GPa
0.580 ksi
Injection molded parts; DIN 53504
Huntsman IROGRAN® CA116-205 TPU-Polyester
Introduction: IROGRAN CA116-205 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-205 is part of the HUNTSMAN film and shee..
300% Modulus 0.00400 GPa
0.580 ksi
ISO 37
Huntsman AVALON® 65 AC Thermoplastic Polyurethane
Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia..
300% Modulus 0.00400 GPa
0.580 ksi
ISO 37
Huntsman AVALON® 65 AE Thermoplastic Polyurethane
Introduction: AVALON 65 AE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AE is part of the AVALON Soft Range and offers a premium soling material for casual, sport..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D412
Lubrizol Advanced Materials PEARLCOAT® DIPP-119 Thermoplastic Polyurethane Elastomer
PEARLCOAT® DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this product..
300% Modulus 0.00400 GPa
0.580 ksi
Taiwan PU Corporation UR60 Polyester Urethane Rubber
UR60 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of ..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
ELASTO UK Dryflex® 400701S SBS Based Material, 70A Hardness, Natural
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
ELASTO UK Dryflex® 402701S SBS Based Material, 70A Hardness, Black
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
ELASTO UK Dryflex® 500700S SEBS Based Material, Unfilled Qualities, 70A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
ELASTO UK Dryflex® 502700S SEBS Based Material, Unfilled Qualities, 70A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
ELASTO UK Dryflex® 600650S SEBS Based Material, Filled Qualities, 65A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
ELASTO UK Dryflex® 600700S SEBS Based Material, Filled Qualities, 70A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
ELASTO UK Dryflex® 600750S SEBS Based Material, Filled Qualities, 75A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
ELASTO UK Dryflex® 602650S SEBS Based Material, Filled Qualities, 65A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
ELASTO UK Dryflex® 602700S SEBS Based Material, Filled Qualities, 70A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
ELASTO UK Dryflex® 602750S SEBS Based Material, Filled Qualities, 75A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
ELASTO UK Dryflex® 660650S SEBS Based Material, Semi-Filled Qualities, 65A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
ELASTO UK Dryflex® 660700S SEBS Based Material, Semi-Filled Qualities, 70A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
ELASTO UK Dryflex® 662650S SEBS Based Material, Semi-Filled Qualities, 65A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D638
ELASTO UK Dryflex® 662700S SEBS Based Material, Semi-Filled Qualities, 70A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D 638
API Megol AM T A SEBS Adhesion Modified Overmolding for Polar Polymers
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..
Copyright © lookpolymers.com All Rights Reserved