Lucas-Milhaupt Silvaloy® 35 Brazing Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name Silvaloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Silvaloy® 35 Brazing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silvaloy 35 is an alloy with a melting range suitable for brazing steel, stainless steel, copper, copper alloys, nickel, nickel alloys or combinations of these metals. It is free-flowing and suited for general purpose work. Its broader melting range is helpful where clearances are not uniform. Typical applications are the joining of ferrous, non-ferrous, and dissimilar metals and alloys with close joint clearances.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 9.29 g/cc
9.29 g/cc
Density 9.30 g/cc
0.336 lb/in³
Thermal Properties Metric English Comments
Melting Point 607.2 - 701.7 °C
1125 - 1295 °F
Solidus 607.2 °C
1125 °F
Liquidus 701.7 °C
1295 °F
Maximum Service Temperature, Air 204 °C
400 °F
continuous
316 °C
600 °F
intermittent
Component Elements Properties Metric English Comments
Cadmium, Cd 17 - 19 %
17 - 19 %
Copper, Cu 25 - 27 %
25 - 27 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 34 - 36 %
34 - 36 %
Zinc, Zn 19 - 23 %
19 - 23 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000626 ohm-cm
0.00000626 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 701.7 - 843 °C
1295 - 1550 °F
Brazing Temperature
Descriptive Properties Value Comments
Color Light Yellow
Electrical Conductivity (% IACS) 27.5