Lucas-Milhaupt Silvaloy® 45 Brazing Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name Silvaloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Silvaloy® 45 Brazing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silvaloy 45 is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining steel, stainless steel, copper, copper alloys, nickel, nickel alloys or combinations of these metals. It has a wide acceptance by industrial users, as well as being included in Federal military specifications on brazing filler metals or alloys. It has a narrow melting range which is not apparent in most brazing operations, making it flow freely though a capillary. Typical applications are the joining of ferrous, non-ferrous, and dissimilar metals and alloys with close joint clearances.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 9.34 g/cc
9.34 g/cc
Density 9.41 g/cc
0.340 lb/in³
Thermal Properties Metric English Comments
Melting Point 607.2 - 618.3 °C
1125 - 1145 °F
Solidus 607.2 °C
1125 °F
Liquidus 618.3 °C
1145 °F
Maximum Service Temperature, Air 204 °C
400 °F
continuous
316 °C
600 °F
intermittent
Component Elements Properties Metric English Comments
Cadmium, Cd 23 - 25 %
23 - 25 %
Copper, Cu 14 - 16 %
14 - 16 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 44 - 46 %
44 - 46 %
Zinc, Zn 14 - 18 %
14 - 18 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000606 ohm-cm
0.00000606 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 618.3 - 760 °C
1145 - 1400 °F
Brazing Temperature
Descriptive Properties Value Comments
Color Light Yellow
Electrical Conductivity (% IACS) 27.6