Lucite International Elvakon® 4494 Low Gloss Acrylic Capstock

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Extruded
Manufacturer Lucite International
Trade Name Elvakon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvakon® 4494 Low Gloss Acrylic Capstock.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable protective coating.Information provided by Lucite International
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 0.40 %
0.40 %
ISO 62
Melt Flow 2.2 g/10 min
2.2 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 74
74
ISO 2039-2
Tensile Strength 29.0 MPa
4210 psi
ISO 527
Elongation at Break 27 %
27 %
ISO 527
Flexural Strength 42.0 MPa
6090 psi
ISO 178
Flexural Modulus 1.90 GPa
276 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 5.30 J/cm²
25.2 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.530 J/cm²
2.52 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C
151 °F
ISO 75A
Vicat Softening Point 69.0 °C
156 °F
ISO 306B
84.0 °C
183 °F
ISO 306A