Material Notes:
Master Bond Polymer System EP21FRSPLV is a two component, room temperature curable, flame resistant compound for potting, encapsulating and casting. EP21FRSPLV has a one to one mix ratio, by weight. Meets UL 94V.O Flame Retardant Specification.
Physical Properties Metric English Comments
Viscosity 25000 - 30000 cP

@Temperature 23.0 °C
25000 - 30000 cP

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
1440 - 2880 min

@Temperature 23.0 °C
24.0 - 48.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Code "A" Red; "B" White
Mix Ratio By Weight 100/100
Set-Up Time, minutes 30-60
At Room Temperature
Users viewing this material also viewed the following: