Master Bond Mastersil 415 One Component Room Temperature Curing, Transparent Silicon

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Master Bond Inc.
Trade Name Mastersil
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond Mastersil 415 One Component Room Temperature Curing, Transparent Silicon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond MasterSil 415 is a ready-to-use, one component high performance silicone elastomer compound for bonding, sealing and protective coatings featuring high transparency. It has a paste consistency and will not sag, slump or run off surfaces. It cures at ambient temperatures to a flexible rubbery solid when exposed to atmospheric moisture.
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Tensile Strength, Yield 2.24 MPa
325 psi
Elongation at Yield 375 %
375 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -121 °C
-185 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Processing Properties Metric English Comments
Cure Time 720 - 1440 min

@Temperature 23.0 °C
12.0 - 24.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Transparent
Set-Up Time, minutes 8-12
At Room Temperature
Viscosity Paste