Micropol Microcene MC123 Metallocene Based Polyethylene Rotational Molding Powder

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Micropol Limited
Trade Name Microcene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Micropol Microcene MC123 Metallocene Based Polyethylene Rotational Molding Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: reduced fusion, compacting, and crystallization times or lower oven temperatures; improved wall thickness control, improved impact resistance; low warpage; better creep resistance. Information provided by Micropol Limited
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792-91
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238-94
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ASTM D2240-86
Tensile Strength, Yield 20.0 MPa
2900 psi
50mm/min; ASTM D638M-89
Flexural Modulus 0.750 GPa
109 ksi
2mm/min; ASTM D790-86
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C
154 °F
ASTM D648-82