Material Notes:
Description: AS33L-07 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications.Key Applications: Bumper fascias, cladding and bodyside moldingInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Melt Flow 22 g/10 min
22 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 44
44
ASTM D785
Tensile Strength, Yield 19.0 MPa
2760 psi
50 mm/min; ASTM D638
Flexural Modulus 1.15 GPa
167 ksi
Tangent; 1.3 mm/min; ASTM D790
Izod Impact, Notched 6.00 J/cm

@Temperature 23.0 °C
11.2 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648