NIZHNEKAMSKNEFTEKHIM PE 2062T (62107) High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer NIZHNEKAMSKNEFTEKHIM Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NIZHNEKAMSKNEFTEKHIM PE 2062T (62107) High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Physical Properties Metric English Comments
Density 0.960 - 0.964 g/cc
0.0347 - 0.0348 lb/in³
Base Resin; ASTM D1505
Melt Flow 6.0 - 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 - 8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
180 - 240 g/10 min

@Load 21.6 kg,
Temperature 190 °C
180 - 240 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
Mechanical Properties Metric English Comments
Flexural Modulus >= 1.50 GPa
>= 218 ksi
ASTM D790
Izod Impact, Notched >= 0.550 J/cm

@Temperature 23.0 °C
>= 1.03 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Users viewing this material also viewed the following: