NIZHNEKAMSKNEFTEKHIM PP 4316M (EP1X35AF) Propylene and Ethylene Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , Polypropylene (PP)
Manufacturer NIZHNEKAMSKNEFTEKHIM Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NIZHNEKAMSKNEFTEKHIM PP 4316M (EP1X35AF) Propylene and Ethylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when PP is produced, processed and PP-made articles are exploited, improved properties contributing to slipping and preventing from film layers sticking, and improved antistatic properties.Information provided by manufacturer
Physical Properties Metric English Comments
Melt Flow 7.0 - 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 - 10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 29.0 MPa
>= 4210 psi
ASTM D638
Elongation at Yield >= 10 %
>= 10 %
ASTM D638
Flexural Modulus >= 1.05 GPa
>= 152 ksi
ASTM D790
Izod Impact, Notched >= 0.350 J/cm

@Temperature 23.0 °C
>= 0.656 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Descriptive Properties Value Comments
Gel Content (pcs./m²) 0
>= 2.5mm
0
(1.5-2.5)mm
3
(0.7-1.5)mm
300
>=0.2mm