NOVA Chemicals Sclair® 2515 MDPE Injection Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 2515 MDPE Injection Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent processability for applications requiring moderate stiffness and improved toughnessExcellent cold temperature impact properties Applications: Ice cream containersHousewares Deep skirt lidsInformation provided by Nova Chemicals
Physical Properties Metric English Comments
Bulk Density 0.580 g/cc
0.0210 lb/in³
Density 0.941 g/cc
0.0340 lb/in³
ASTM D792
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 37.0 cm
14.6 in
NOVA
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D2240
Tensile Strength, Yield 20.0 MPa
2900 psi
50 mm/min; ASTM D638
Elongation at Break 16 %
16 %
50 mm/min; ASTM D638
Flexural Modulus 0.760 GPa
110 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 114 °C
237 °F
ASTM D1525