Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NYCOA 27/300SR Glass Filled Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Fiber Filled, Flame Retardant
Manufacturer NYCOA, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NYCOA 27/300SR Glass Filled Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% glass filled, flame retardant to UL 94 H-B nylon 6Information provided by NYCOA, Inc.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Water Absorption 1.7 %
1.7 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 175 MPa
25400 psi
ASTM D638
Elongation at Break >= 6.0 %
>= 6.0 %
ASTM D638
Flexural Yield Strength 240 MPa
34800 psi
ASTM D790
Flexural Modulus 8.00 GPa
1160 ksi
ASTM D790
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ASTM D789
Flammability, UL94 HB

@Thickness 0.700 mm
HB

@Thickness 0.0276 in
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
Rear Barrel Temperature 225 °C
437 °F
Middle Barrel Temperature 230 °C
446 °F
Front Barrel Temperature 250 °C
482 °F
Nozzle Temperature 250 °C
482 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 76.0 °C
169 °F
Users viewing this material also viewed the following: