Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Network Polymers MS 150 Styrene Methyl Methacrylate Terpolymer

Category Polymer , Thermoplastic , Acrylic (PMMA) , Polystyrene (PS) , Styrene/Methyl Methacrylate Copolymer (SMMA)
Manufacturer Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers MS 150 Styrene Methyl Methacrylate Terpolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Water Absorption 0.10 %
0.10 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Melt Flow 3.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.42 MPa
4992 psi
chs 2 in/min; ASTM D638
Elongation at Break 31 %
31 %
chs 2 in/min; ASTM D638
Modulus of Elasticity 2.20 GPa
319 ksi
ASTM D638
Flexural Modulus 1.83 GPa
266 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
0.125 inch bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C
181 °F
Unannealed/Conditioned 48 hours at 23°C; ASTM D648
Vicat Softening Point 97.0 °C
207 °F
ASTM D1525
Optical Properties Metric English Comments
Transmission, Visible 89 %
89 %
ASTM D1003
Copyright © lookpolymers.com All Rights Reserved