Network Polymers NPP 30-007W

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers NPP 30-007W.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 0.60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 35.9 MPa
5200 psi
2 in per min; ASTM D638
Elongation at Yield 12 %
12 %
chs 2 in/min; ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
Test Method A (0.125 in bar); ASTM D256