Nilit Polynil® P120 Medium Viscosity Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Nilit
Trade Name Polynil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit Polynil® P120 Medium Viscosity Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Medium viscosityApplication: MonofilamentInformation provided by NILIT.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Viscosity Measurement 120
120
relative viscosity (formic acid); ASTM D789
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Tensile Modulus 3.00 GPa
435 ksi
ASTM D638
Flexural Strength 115 MPa
16700 psi
ASTM D790
Flexural Modulus 2.70 GPa
392 ksi
ASTM D790
Izod Impact, Notched (ISO) 6.09 kJ/m²
2.90 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ASTM D648