Material Notes:
Description: Nylene® 9110 is an unfilled specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Flexural Modulus 2.03 GPa
295 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 214 °C
418 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 174 °C
345 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.2 °C
144 °F
ASTM D648