Nylene® 9543 , 43% Glass Reinforced Nylon 6/12

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Glass Fiber Filler
Manufacturer Nylene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® 9543 , 43% Glass Reinforced Nylon 6/12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nylene® 9543 s a 43% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 165 MPa
24000 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 224 °C
435 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648