Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 165 MPa | 24000 psi | ASTM D638 |
Nylene® 9110 G43 , 43% Glass Reinforced Nylon 6/10 Description: Nylene® 9110 G43 is a 43% glass fiber reinforced specialty nylon. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | ASTM D638 |
Nylene® 9543 , 43% Glass Reinforced Nylon 6/12 Description: Nylene® 9543 s a 43% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resour.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | ASTM D638 |
Custom Resins Vexel™ E20GF45 FR , 45% Glass Reinforced, Flame Retardant PET
(discontinued **) Description: Vexel™ E20GF45 FR is a 45% glass fiber reinforced, flame retardant PET. Information provided by Custom Resins. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® NL-23CF/000 Nylon 6/12, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | ASTM D638 |
Global GPEI-230 30% Glass Filled Reinforced Polyetherimide Alloy Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | ASTM D638 |
Techmer ES Plaslube® J-3/30/TF/13/SI/2 Nylon 6, 30% GFR, 13% PTFE, 2% Silicone Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/16" to 1/4" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | |
AIM 35.7Sn/35.7Pb/28.6Bi Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/8" to 1" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |