Overview of materials for Nylon 11 with 40% Glass Fiber Filler

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11 with 40% Glass Fiber Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 11 with 40% Glass Fiber Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.35 - 1.42 g/cc
0.0488 - 0.0513 lb/in³
Average value: 1.38 g/cc Grade Count:4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 82.7 - 146 MPa
12000 - 21200 psi
Average value: 114 MPa Grade Count:4
Elongation at Break 2.00 - 4.00 %
2.00 - 4.00 %
Average value: 3.50 % Grade Count:4
Modulus of Elasticity 8.27 - 12.4 GPa
1200 - 1800 ksi
Average value: 10.2 GPa Grade Count:4
Charpy Impact Unnotched 7.29 - 7.50 J/cm²

@Temperature -30.0 - -30.0 °C
34.7 - 35.7 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.39 J/cm² Grade Count:2
Charpy Impact, Notched 0.980 - 1.02 J/cm²

@Temperature -30.0 - -30.0 °C
4.66 - 4.85 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.00 J/cm² Grade Count:2
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
Grade Count:4