Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 12.4 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.765 - 12.4 GPa
111 - 1800 ksi
Average value: 8.36 GPa Grade Count:47
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Modulus of Elasticity 2.90 - 12.4 GPa
420 - 1790 ksi
Average value: 8.85 GPa Grade Count:5
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va..
Modulus of Elasticity 5.52 - 12.4 GPa
800 - 1800 ksi
Average value: 9.72 GPa Grade Count:16
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E..
Modulus of Elasticity 1.10 - 12.4 GPa
160 - 1800 ksi
Average value: 3.02 GPa Grade Count:64
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Modulus of Elasticity 8.27 - 12.4 GPa
1200 - 1800 ksi
Average value: 10.2 GPa Grade Count:4
Overview of materials for Nylon 11 with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are includ..
Modulus of Elasticity 5.50 - 12.4 GPa
798 - 1800 ksi
Average value: 10.4 GPa Grade Count:21
Overview of materials for Polycarbonate, 40% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E..
Modulus of Elasticity 3.79 - 12.4 GPa
550 - 1800 ksi
Average value: 7.63 GPa Grade Count:8
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a..
Modulus of Elasticity 3.59 - 12.4 GPa
520 - 1800 ksi
Average value: 8.31 GPa Grade Count:76
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..