Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.30 - 7.50 J/cm² @Temperature -30.0 - -20.0 °C |
10.9 - 35.7 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 4.35 J/cm² Grade Count:21 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Charpy Impact Unnotched | 0.250 - 7.50 J/cm² @Temperature -30.0 - -20.0 °C |
1.19 - 35.7 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 4.47 J/cm² Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Charpy Impact Unnotched | 7.00 - 7.50 J/cm² @Temperature -30.0 - -30.0 °C |
33.3 - 35.7 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.17 J/cm² Grade Count:6 |
Overview of materials for Nylon 63, 35% Glass-Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Charpy Impact Unnotched | 7.29 - 7.50 J/cm² @Temperature -30.0 - -30.0 °C |
34.7 - 35.7 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.39 J/cm² Grade Count:2 |
Overview of materials for Nylon 11 with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are includ.. |
|||
Charpy Impact Unnotched | 2.50 - 7.50 J/cm² | 11.9 - 35.7 ft-lb/in² | Average value: 5.09 J/cm² Grade Count:9 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Charpy Impact Unnotched | 1.60 - 7.50 J/cm² | 7.61 - 35.7 ft-lb/in² | Average value: 4.16 J/cm² Grade Count:7 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Charpy Impact Unnotched | 3.50 - 7.50 J/cm² @Temperature -40.0 - -30.0 °C |
16.7 - 35.7 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 5.25 J/cm² Grade Count:10 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |