Overview of materials for Nylon, Barrier Film Copolymer

Category Polymer , Film , Thermoplastic , Nylon , Nylon, Barrier Film Copolymer
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon, Barrier Film Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Barrier Film Copolymer". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.13 - 1.19 g/cc
0.0408 - 0.0430 lb/in³
Average value: 1.16 g/cc Grade Count:9
Viscosity 200000 - 200000 cP

@Temperature 300 - 300 °C
200000 - 200000 cP

@Temperature 572 - 572 °F
Average value: 200000 cP Grade Count:1
200000 - 200000 cP

@Shear Rate 100 - 100 1/s
200000 - 200000 cP

@Shear Rate 100 - 100 1/s
Average value: 200000 cP Grade Count:1
Thermal Properties Metric English Comments
Melting Point 218 - 220 °C
424 - 428 °F
Average value: 219 °C Grade Count:6
Glass Transition Temp, Tg 125 - 127 °C
257 - 261 °F
Average value: 126 °C Grade Count:3
Processing Properties Metric English Comments
Drying Temperature 80.0 °C
176 °F
Average value: 80.0 °C Grade Count:4