Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.18 - 1.19 g/cc | 0.0426 - 0.0430 lb/in³ | Polymerized; ASTM D792 |
Proto3000 Objet FullCure720 Transparent Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Density | 1.18 - 1.19 g/cc | 0.0426 - 0.0430 lb/in³ | Polymerized; ASTM D792 |
Proto3000 Objet VeroBlue FullCure840 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Density | 1.04 - 1.19 g/cc | 0.0376 - 0.0430 lb/in³ | Average value: 1.05 g/cc Grade Count:99 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Density | 1.15 - 1.19 g/cc | 0.0415 - 0.0430 lb/in³ | Average value: 1.18 g/cc Grade Count:17 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
Density | 1.15 - 1.19 g/cc | 0.0415 - 0.0430 lb/in³ | Average value: 1.18 g/cc Grade Count:11 |
Overview of materials for Acrylic, High Flow, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app.. |
|||
Density | 1.13 - 1.19 g/cc | 0.0408 - 0.0430 lb/in³ | Average value: 1.16 g/cc Grade Count:9 |
Overview of materials for Nylon, Barrier Film Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Barrier Film Copolymer". Each property range of values reported is minimum and maximum values of .. |
|||
Density | 1.11 - 1.19 g/cc | 0.0403 - 0.0429 lb/in³ | |
Lord Adhesives 5 Mix-In Accelerator for 200, 400, 500 Series Lord Adhesives 5 Mix-In Accelerator for 200, 400, 500 SeriesLord Accelerator 5 is a mix-in accelerator for Lord 200, 400, and 500 series acrylic adhesives. Use at 20:1 ratio. |
|||
Density | 1.16 - 1.19 g/cc | 0.0419 - 0.0430 lb/in³ | |
Solvay GLOKILL® PQ60 Surfactant Description: Algicide and biocide for swimming poolIdentification: POLYQUARTERNARY AMMONIUM CHLORIDE, AQUEOUS SOLUTIONCAS: 25988 – 97 – 0Available in: EuropeFunction: Algaecide for use in .. |
|||
Density | 1.12 - 1.19 g/cc | 0.0405 - 0.0428 lb/in³ | |
CMT Materials HYTAC® B Solid Polymer Tooling Material Sometimes, finer plug assist details are required which are not obtainable or maintainable with syntactic foam plugs. For these high detail applications, where high toughness and easy machinability .. |
|||
Density | 1.15 - 1.19 g/cc | 0.0415 - 0.0430 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 30 Flexible PVC, Injection Molding, Lead Free Scooter handle-bar grip |
|||
Density | 1.15 - 1.19 g/cc | 0.0415 - 0.0430 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 57 Medical Flexible PVC, Extrusion Tubolar apparatus and peristaltic pump segments |
|||
Density | 1.15 - 1.19 g/cc | 0.0415 - 0.0430 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 56/B Flexible PVC, Extrusion Modified with Rubber Hydrocarbon resisting tubes |
|||
Density | 1.15 - 1.19 g/cc | 0.0415 - 0.0430 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 60/A Flexible PVC, Transparent Extrusion Profiles, UL Class V2 |
|||
Density | 1.14 - 1.19 g/cc | 0.0412 - 0.0430 lb/in³ | Part A |
3M Scotch-Weld™ DP600 Concrete Repair and Self-Leveling 3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600 is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a trigg.. |
|||
Density | 1.15 - 1.19 g/cc | 0.0415 - 0.0430 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 564D Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Density | 1.14 - 1.19 g/cc | 0.0412 - 0.0430 lb/in³ | Part A |
3M Scotch-Weld™ DP600NS Concrete Repair and Self-Leveling 3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600NS is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a tri.. |
|||
Density | 1.14 - 1.19 g/cc | 0.0412 - 0.0430 lb/in³ | Part A |
3M Scotch-Weld™ DP601 Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon.. |
|||
Density | 1.14 - 1.19 g/cc | 0.0412 - 0.0430 lb/in³ | Part A |
3M Scotch-Weld™ DP601NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon.. |
|||
Density | 0.913 - 1.19 g/cc | 0.0330 - 0.0430 lb/in³ | Average value: 0.940 g/cc Grade Count:29 |
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Masterbatch Grade". Each property range of values reported is minimum a.. |
|||
Density | 1.13 - 1.19 g/cc | 0.0408 - 0.0430 lb/in³ | Average value: 1.18 g/cc Grade Count:37 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Density | 1.04 - 1.19 g/cc | 0.0376 - 0.0430 lb/in³ | Average value: 1.15 g/cc Grade Count:125 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Density | 1.18 - 1.19 g/cc | 0.0426 - 0.0430 lb/in³ | Average value: 1.19 g/cc Grade Count:10 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Density | 1.15 - 1.19 g/cc | 0.0415 - 0.0430 lb/in³ | Average value: 1.18 g/cc Grade Count:14 |
Overview of materials for Acrylic, Optical Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 1.11 - 1.19 g/cc | 0.0401 - 0.0430 lb/in³ | Average value: 1.18 g/cc Grade Count:132 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |