Parker Chomerics CHO-SHIELD® 596 A/B Silver-Epoxy Coating

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Electrically Conductive , Filled/Reinforced Thermoset
Manufacturer Parker Chomerics
Trade Name CHO-SHIELD®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SHIELD® 596 A/B Silver-Epoxy Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silver-Epoxy Coating. This is a two-component, silver bearing, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric substrate. It is also useful for coating flanges for salt spray corrosion protection when mounting an electrically conductive gasket between the surfaces.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 0.060 ohm
<= 0.060 ohm
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 121 °C
1.00 hour

@Temperature 250 °F
360 min

@Temperature 65.0 °C
6.00 hour

@Temperature 149 °F
10100 min

@Temperature 24.0 °C
168 hour

@Temperature 75.2 °F
Pot Life 480 min

@Temperature 24.0 °C
480 min

@Temperature 75.2 °F
480 min

@Temperature 23.9 °C
480 min

@Temperature 75.0 °F
Shelf Life 9.00 Month
9.00 Month
@ 75°F
9.00 Month

@Temperature 24.0 °C
9.00 Month

@Temperature 75.2 °F
Descriptive Properties Value Comments
Binder Epoxy
Consistency Medium Fluid
Filler Ag
Mix Ratio 100:37
Spraying Viscosity, #2 Zahn Cup 19 - 26 sec
Theoretical Yield 50 ft2/lb
1.5 mil