Permabond 795 Cyanoacrylate, Surface insensitive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond 795 Cyanoacrylate, Surface insensitive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PERMABOND® 795 is a moderate viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers are also rapidly bonded. The fast cure minimizes the occurrence of frosting and fogging. Cyanoacrylate adhesives are single component adhesives that polymerize rapidly when pressed into a thin film between parts. The moisture adsorbed on the surface initiates the curing of the adhesive. Strong bonds are developed extremely fast and on a great variety of materials. These properties make PERMABOND® cyanoacrylates the ideal adhesives for high speed production lines. Features & Benefits: Extremely fast setting Rapid development of high strength Ease of use – no mixing or heat cure Surface insensitive 100% reactive, no solvents Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 500 cP

@Temperature 25.0 °C
500 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C
35.6 - 44.6 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ISO 868
Adhesive Bond Strength 18.0 - 22.0 MPa
2610 - 3190 psi
Steel, Shear; ISO 4587
Impact 3.0 - 5.0
3.0 - 5.0
kJ/m<sup>2</sup> Adhesive Impact Strength; ASTM D950
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Constant 2.5

@Frequency 10000 Hz
2.5

@Frequency 10000 Hz
Dielectric Strength 25.0 kV/mm
635 kV/in
Processing Properties Metric English Comments
Cure Time 0.0667 min
0.00111 hour
Steel, handling time
0.0667 min
0.00111 hour
Buna N Rubber, handling time
0.0667 min
0.00111 hour
Phenolic, handling time
1440 min
24.0 hour
full strength
Descriptive Properties Value Comments
Appearance Colorless
Uncured
Maximum Gap Fill (mm) 0.18
Strength Retention 10% at 150°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 100°C
Relative to 0°C
55% at -50°C
Relative to 0°C
90% at 50°C
Relative to 0°C