Material Notes:
Petromont HDPE 1202 is a high-density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for use in the blow moulding of large parts such as shipping containers ranging in sizes from 19 to 210 litres (5 to 55 gallons). It is also used in automotive fuel tanks, jerrycans, sleds, floating docks, etc.Petromont HDPE 1202 is a high molecular weight hexene modified resin with a broad molecular weight distribution offering excellent parison stability, combined with excellent stress cracking resistance, toughness and good rigidity. It also has excellent resistance to most chemicals.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 2000 hour
>= 2000 hour
F<sub>50</sub>; ASTM D1693-B
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
F<sub>50</sub>; ASTM D1693-B
Melt Flow 0.080 g/10 min
0.080 g/10 min
I<sub>2</sub>; ASTM D1238
10 g/10 min
10 g/10 min
I<sub>21</sub>; ASTM D238
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.1 MPa
5090 psi
ASTM D638
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
ASTM D790
Izod Impact, Notched >= 2.13 J/cm
>= 3.99 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Process Blow Molding