Plaskolite Optix® CP - 86 UVA General Purpose Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, General Purpose, Molded , Acrylic, Optical Grade, Molded
Manufacturer Plaskolite
Trade Name Optix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite Optix® CP - 86 UVA General Purpose Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskolite, Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D-955
Melt Flow 1.6 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.6 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength 72.4 MPa
10500 psi
ASTM D-638
Elongation at Break 4.5 %
4.5 %
ASTM D-638
Modulus of Elasticity 3.65 GPa
530 ksi
ASTM D-638
Flexural Strength 117 MPa
17000 psi
ASTM D-790
Izod Impact, Notched 0.160 J/cm

@Thickness 6.35 mm
0.300 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Gardner Impact 0.226 J

@Thickness 3.17 mm
0.167 ft-lb

@Thickness 0.125 in
Falling Weight; ASTM D-3029 GB
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C
33.3 µin/in-°F
ASTM D-696
Maximum Service Temperature, Air 90.0 °C
194 °F
UL-746 ABC
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
ASTM D-648
Vicat Softening Point 113 °C
236 °F
ASTM D-1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
ASTM D-1003
Transmission, Visible 92 %
92 %
ASTM D-1003
Descriptive Properties Value Comments
3-Year Weathering Listed
SAE J 576 (AMECA)