Plaskolite Optix® SG Sign Grade Acrylic Sheet

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Optical Sheet
Manufacturer Plaskolite
Trade Name Optix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite Optix® SG Sign Grade Acrylic Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in unlimited lengths - no seams in finished products.Data provided by the manufacturer, Plaskolite, Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 96
96
Method A; ASTM D785
Tensile Strength, Yield 72.0 MPa
10400 psi
ASTM D638
Tensile Modulus 3.00 GPa
435 ksi
ASTM D638
Flexural Yield Strength 110 MPa
16000 psi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
0.200 J/cm

@Temperature -18.0 °C
0.375 ft-lb/in

@Temperature -0.400 °F
ASTM D256
Gardner Impact 0.500 J
0.369 ft-lb
reported as J/cm; ASTM D3029-GB, unpainted
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C

@Temperature -18.0 - 38.0 °C
30.0 µin/in-°F

@Temperature -0.400 - 100 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C
208 °F
annealed; ASTM D648
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
ASTM D1003
Transmission, Visible 92 %
92 %
ASTM D1003
Processing Properties Metric English Comments
Processing Temperature 160 °C
320 °F
Optimal Thermoforming temperature for sheet 0.25-1.0 cm (0.10-0.39 in)