Material Notes:
FeaturesPA 6 for injection moulding, chemically strengthened with 30% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electro tools, hobby tools, gears, covers of electric appliances, cooling screws of blowers, electromotors, carrying parts in the automotive industry, gas pedals, etc. Delivered in natural mode and in the full RAL color scale.Application: Injection MouldingInformation Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
STN 64 0111
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
STN 64 0808
Linear Mold Shrinkage, Transverse 0.0106 cm/cm
0.0106 in/in
STN 64 0808
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 170 MPa
24700 psi
STN EN ISO 527-2
Elongation at Break 3.0 %
3.0 %
STN EN ISO 527-2
Tensile Modulus 9.60 GPa
1390 ksi
STN EN ISO 527-2
Flexural Strength 235 MPa
34100 psi
STN EN ISO 178
Flexural Modulus 8.40 GPa
1220 ksi
STN EN ISO 178
Charpy Impact Unnotched 7.50 J/cm²

@Temperature -20.0 °C
35.7 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
8.50 J/cm²

@Temperature 23.0 °C
40.4 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched 1.10 J/cm²

@Temperature -20.0 °C
5.23 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
DSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 212 °C
414 °F
STN EN ISO 75/A
Vicat Softening Point 221 °C
430 °F
B; STN EN ISO 306
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
STN IEC 60695-2-10
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+13 ohm-cm
5.00e+13 ohm-cm
STN IEC 60093
Surface Resistance 8.00e+13 ohm
8.00e+13 ohm
STN IEC 60093
Dielectric Strength 20.0 kV/mm
508 kV/in
STN IEC 60243
Comparative Tracking Index 575 V
575 V
STN 34 6468
Processing Properties Metric English Comments
Melt Temperature 250 - 280 °C
482 - 536 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
STN EN ISO 960
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi