Plastics Group Polifil® GFABS-30 30% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® GFABS-30 30% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: FirearmsAutomotiveHousehold appliancesStandard processing techniques are applicable. Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ASTM D792
Filler Content 30 %
30 %
ASTM D2584
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 1.59 mm
0.0020 in/in

@Thickness 0.0625 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength at Break 89.6 MPa
13000 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Tensile Modulus 6.27 GPa
910 ksi
ASTM D638
Flexural Strength 116 MPa
16800 psi
ASTM D790
Flexural Modulus 6.41 GPa
930 ksi
Tangent; ASTM D790
Compressive Strength 103 MPa
15000 psi
ASTM D695
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
At 73°F; ASTM D256
Izod Impact, Unnotched 3.36 J/cm
6.30 ft-lb/in
At 73°F; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 17.0 µm/m-°C

@Temperature 20.0 °C
9.44 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 60.0 °C
140 °F
Continuous use; UL 746B
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ASTM D648
Flammability, UL94 HB
HB
Class 1/16
Oxygen Index <= 27 %
<= 27 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.4

@Frequency 10000 Hz
3.4

@Frequency 10000 Hz
ASTM D150
Dielectric Strength 18.9 kV/mm
480 kV/in
ASTM D149
Dissipation Factor 0.0090

@Frequency 10000 Hz
0.0090

@Frequency 10000 Hz
ASTM D150
Arc Resistance 80 sec
80 sec
Dry; ASTM D495
Users viewing this material also viewed the following: