Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastics Group Polifil® RP-ABS Acrylonitrile-Butadiene Styrene, Standard Version

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® RP-ABS Acrylonitrile-Butadiene Styrene, Standard Version.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® RP- Acrylonitrile-Butadiene Styrene is a styrenic resin with improved toughness and heat resistance versus HIPS grades. ABS exhibits high gloss, low shrinkage, and good dimensional stability. ABS is widely used in injection molding of appliances, furniture, and automotive parts. ABS also has high melt strength suitable for the production of extruded sheet, some of considerable size and thickness. Applications include panels for large appliances and thermoformed items such as hot tubs and recreational vehicle parts. Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hours; ASTM D570
Melt Flow 4.0 - 8.0 g/10 min
4.0 - 8.0 g/10 min
230/3.8; May be specified; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Modulus 2.14 GPa
310 ksi
1% Secant; ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 98.9 °C
210 °F
ASTM D648