Material Notes:
Symbol according to ISO 1043/1: PC+ABS Similar to KOBLEND PCA 638 with an improved fluidity, suitable to mould complex items. Unfilled. Suitable for Injection Molding. Supplied as pellets.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Water Absorption 0.60 %
0.60 %
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 260 °C
18 g/10 min

@Load 11.0 lb,
Temperature 500 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 4.5 %
4.5 %
50 mm/min
Tensile Modulus 2.10 GPa
305 ksi
1 mm/min
Izod Impact, Unnotched NB
NB
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Izod Impact, Notched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 75.0 µm/m-°C

@Temperature 20.0 °C
41.7 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 124 °C
255 °F
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
217 °F
Vicat Softening Point 120 °C
248 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Constant 2.7

@Frequency 1e+6 Hz
2.7

@Frequency 1e+6 Hz
2.8

@Frequency 100 Hz
2.8

@Frequency 100 Hz
Dielectric Strength 27.0 kV/mm
686 kV/in
Dissipation Factor 0.0040

@Frequency 100 Hz
0.0040

@Frequency 100 Hz
0.0070

@Frequency 1e+6 Hz
0.0070

@Frequency 1e+6 Hz
Comparative Tracking Index 300 V
300 V