Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa SINKRAL PD C823 ABS, Impact Grade  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa SINKRAL PD C823 ABS, Impact Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-35-15 Injection moulding grade, exhibiting very high impact resistance, even at low temperatures. Applications: automotive industry, where parts must withstand high mechanical stress.Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains lubricant and release agent.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Water Absorption 1.0 %
1.0 %
Moisture Absorption at Equilibrium 0.20 %
0.20 %
Humidity Absorption
Melt Flow 4.5 g/10 min

@Load 10.0 kg,
Temperature 220 °C
4.5 g/10 min

@Load 22.0 lb,
Temperature 428 °F
cm³/10 min
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Strength 30.0 kV/mm
762 kV/in
Comparative Tracking Index 600 V
600 V