PolyOne Edgetek® AT-30GF/000 FDA Acetal-Copolymer, Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® AT-30GF/000 FDA Acetal-Copolymer, Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.62 g/cc
1.62 g/cc
ASTM D792
Water Absorption 0.0080 %
0.0080 %
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0035 cm/cm
0.0030 - 0.0035 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.8 MPa
11000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 6.89 GPa
1000 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Processing Properties Metric English Comments
Melt Temperature 210 - 238 °C
410 - 460 °F
Molding
Mold Temperature 54.4 - 71.1 °C
130 - 160 °F
Drying Temperature 71.1 °C
160 °F
Dry Time 2 hour
2 hour
Descriptive Properties Value Comments
Product Form Pellets