Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylac® GP74G20 ABS, 20% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR QD 818.Y001 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AT-15GF/10T Acetal-Copolymer, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 IM C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Additive: Impact ModifierFeatures: Conductive and Impact ModifiedAppearance: BlackInformation provided by TP.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES Electrablend® PPS 06000 Availability: North AmericaForms: PelletsFiller/Reinforcement: Metallic FlakeFeatures: Electrically ConductiveInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES Electrablend® TPX-PC-02071 Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF/M15 A1 BK 15% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 15% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized Appearance: BlackInformation provided by TP Compo.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GB20 L BK 20% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES HiFill® PET GF15 IM 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D412 |
Saint-Gobain COHRlastic® CF1869 Thermally Conductive Silicone Coated Fabric Description: Conductive silicones expand the use of our products into the electronic assembly market. By the use of special fillers, silicone can be made thermally or electrically conductive. CF1869.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES Luriblend® PC GF30 TS15 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Com.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES Plastiblend® PA6/6 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Low Viscosity and LubricatedProcessing Method: Injection MoldingInformation provided by TP .. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES Plastiblend® PA6/ABS 1120 GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: Natural ColorInformation p.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES Plastiblend® TPX-HTN-000CA Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES Statiblend® PA6/6 02013 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforAdditive: Impact ModifierFeatures: Conductive and Impact ModifiedUL File Number: E157318TPCI# 1039101Informati.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES HiFill® PP CO GF43 CC 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES Luriblend® POM CO CF10 TL10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Lubricated and CopolymerUL File: E157318Information provided b.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Ensinger Tecast Vekton™ 6XAU High Heat Cast Nylon 6 (PA6) VEKTON® 6XAU is a high heat weather resistant cast nylon 6 with superior fatigue-resistant and bearing properties.General Vekton® Cast Nylon Information: VEKTON cast nylon, available in a variety .. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 75.8 - 427 MPa | 11000 - 62000 psi | |
Chicago Extruded Metals BioBrass® UNS C22600 Copper-Zinc Alloy Finished product available as bar or wire.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metal.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Ensinger Tecast Vekton™ 6PAL Oil-Filled Cast Nylon 6 (PA6) Tecast® 6PAL is used in applications requiring excellent bearing and wear properties where external lubrication is difficult or impractical.General Tecast® Cast Nylon Information: Tecast cast nylo.. |
|||
Tensile Strength, Yield | 75.8 MPa @Temperature 0.000 °C |
11000 psi @Temperature 32.0 °F |
ASTM D638 |
Celanese CELANEX 2002 PBT, Unfilled Celanex 2002 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002 ia a medium flow material.Information provide.. |
|||
Tensile Strength, Yield | 75.8 MPa @Temperature 0.000 °C |
11000 psi @Temperature 32.0 °F |
ASTM D638 |
Celanese CELANEX 2002-2 PBT, Unfilled Celanex 2002-2 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-2 ia a medium flow material that contains a.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Asahi Kasei Thermylene® P1-35FM-Y942 35% Glass Fiber/Mineral Reinforced Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-30FG-0602 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-30FG-0709 30% Fiber Glass Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Asahi Kasei Thermylene® P7-20FG-0610 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Polymer Resources PPX-FRG10 Modified PPO, UL 94 V-1, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |