Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
15 sec; ASTM D2240
Tensile Strength, Yield 11.0 MPa
1600 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 370 %
370 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
Oxygen Index 21 %

@Thickness 1.91 mm
21 %

@Thickness 0.0752 in
ASTM D2863
Processing Properties Metric English Comments
Melt Temperature 155 - 165 °C
311 - 329 °F
Descriptive Properties Value Comments
Agency Ratings UL QMFZ2
Appearance Clear/Transparent
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Retention of Tensile Elongation 80%
136°C, 1.91 mm; 168 hr, UL Standard
Retention of Tensile Strength 110%
136°C, 1.91 mm; 168 hr, UL Standard
RoHS Compliance RoHS Compliant
Uses Cable Jacketing
Flexible Cord Jacketing
Wire & Cable Applications