Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYfill PPC 20000 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Polykemi AB
Trade Name POLYfill
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYfill PPC 20000 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ISO 1183
Linear Mold Shrinkage 0.015 - 0.018 cm/cm
0.015 - 0.018 in/in
With Flow; ISO 2577
0.015 - 0.018 cm/cm
0.015 - 0.018 in/in
Across Flow; ISO 2577
Melt Index of Compound 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 21.0 MPa
<= 3050 psi
ISO/R527
Flexural Modulus 0.850 GPa

@Temperature 23.0 °C
123 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.800 J/cm²

@Temperature -20.0 °C
3.81 ft-lb/in²

@Temperature -4.00 °F
ISO 179
5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
120°C/h; ISO 75/1
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Glow Wire Test 650 °C

@Thickness 2.00 mm
1200 °F

@Thickness 0.0787 in
IEC 695-2-1
Users viewing this material also viewed the following: