Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB SCANMID 6 B22^ E F20 Nylon 6, Glass Fiber Reinforced, Modified

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer Polykemi AB
Trade Name SCANMID 6
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB SCANMID 6 B22^ E F20 Nylon 6, Glass Fiber Reinforced, Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
Filler Content 20 %
20 %
±2%; Polykemi
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
With Flow; ISO 2577
0.0090 cm/cm
0.0090 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 130 MPa
<= 18900 psi
ISO/R527
Elongation at Break 4.0 %
4.0 %
ISO/R527
Flexural Strength <= 200 MPa
<= 29000 psi
ISO 178
Flexural Modulus 6.40 GPa

@Temperature 23.0 °C
928 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
120°C/h; ISO 75/1
Vicat Softening Point 200 °C

@Load 5.001 kg
392 °F

@Load 11.03 lb
50°C/h; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Glow Wire Test 650 °C

@Thickness 2.00 mm
1200 °F

@Thickness 0.0787 in
IEC 695-2-1
Users viewing this material also viewed the following: