Material Notes:
Information provided by PolyPlastics.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ISO 527-1, 2
Elongation at Break 33 %
33 %
ISO 527-1, 2
Tensile Modulus 2.70 GPa
392 ksi
ISO 527-1, 2
Flexural Strength 87.0 MPa
12600 psi
ISO 178
Flexural Modulus 2.50 GPa
363 ksi
ISO 178
Charpy Impact, Notched 0.550 J/cm²
2.62 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75-1, 2
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
IEC 60093
Dielectric Strength 19.0 kV/mm
483 kV/in
IEC 60243-1
Comparative Tracking Index >= 600 V
>= 600 V
IEC 60112