Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram PlusTek PD300G5 Nylon 12 for Injection Molding, 25% Glass-Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 30% Glass Fiber Filled
Manufacturer Polyram
Trade Name PlusTek
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PD300G5 Nylon 12 for Injection Molding, 25% Glass-Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
25% Glass-fiber reinforced Nylon 12, heat stabilized and hydrolysis resistant for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Water Absorption at Saturation 1.4 %
1.4 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Tensile Modulus 7.00 GPa
1020 ksi
ISO 527
Flexural Strength 150 MPa
21800 psi
ISO 178
Flexural Modulus 5.00 GPa
725 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 175 °C
347 °F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 177 °C
351 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 163 °C
325 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Copyright © lookpolymers.com All Rights Reserved