Material Notes:
Fast cycle polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
DIN 53479
Water Absorption 8.5 %
8.5 %
DIN 53495
Moisture Absorption at Equilibrium 2.8 %
2.8 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM-D785
Tensile Strength, Yield 90.0 MPa
13100 psi
ASTM-D638
Elongation at Break 10 %
10 %
ASTM-D638
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM-D790
Izod Impact, Notched 0.450 J/cm

@Temperature 23.0 °C
0.843 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
Maximum Service Temperature, Air 70.0 °C
158 °F
Continuous Use
180 °C
356 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
DIN 53461
Flammability, UL94 V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in