Polyram RamOfin PPC300S4BK10 Polypropylene, 20% Glass beads

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Glass Bead Filled
Manufacturer Polyram
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamOfin PPC300S4BK10 Polypropylene, 20% Glass beads.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% glass beads reinforced polypropylene copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
DIN 53479
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
ASTM-D638
Elongation at Break >= 100 %
>= 100 %
ASTM-D638
Tensile Modulus 1.319 GPa
191.3 ksi
ASTM-D790
Flexural Strength 25.0 MPa
3630 psi
ASTM D790
Flexural Modulus 1.03 GPa
149 ksi
ASTM-D790
Izod Impact, Notched 0.620 J/cm

@Temperature 23.0 °C
1.16 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 167.7 °C
333.9 °F
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in