Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamOfin PPC370B73 Polypropylene, 73% Mineral Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamOfin PPC370B73 Polypropylene, 73% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
73% mineral filled polypropylene for heavy density injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 2.20 g/cc
0.0795 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM-D638
Elongation at Break 45 %
45 %
ASTM-D638
Tensile Modulus 1.70 GPa
247 ksi
ASTM-D790
Flexural Strength 18.0 MPa
2610 psi
ASTM D790
Flexural Modulus 2.22 GPa
322 ksi
ASTM-D790
Izod Impact, Notched 1.00 J/cm

@Temperature 23.0 °C
1.87 ft-lb/in

@Temperature 73.4 °F
ASTM-D256