Material Notes:
Flame retardant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
DIN 53479
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM-D638
Elongation at Break 200 %
200 %
ASTM-D638
Tensile Modulus 1.20 GPa
174 ksi
ASTM-D790
Flexural Strength 35.0 MPa
5080 psi
ASTM D790
Flexural Modulus 1.50 GPa
218 ksi
ASTM-D790
Izod Impact, Notched 0.850 J/cm

@Temperature 23.0 °C
1.59 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
Glow Wire Test 850 °C
1560 °F