Precision Polymer Engineering E80K Ethylene Propylene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering E80K Ethylene Propylene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose, peroxide cured, Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet ASTM D2000/SAE J200 line call-out MCA810, A25, B35, F17.Applications: Excellent water and steam resistance with good compression set properties. Better heat and chemical resistance than sulphur cured EPDM. Not mineral oil resistant.
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
°IRHD; ASTM D1415
90
90
°IRHD, +10 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 8.00 MPa
1160 psi
-20% change after 70 hours @ 100°C; ASTM D412
10.0 MPa
1450 psi
ASTM D412
Elongation at Break 90.0 %
90.0 %
-40% change after 70 hours @ 100°C; ASTM D412
150 %
150 %
ASTM D412
Compression Set 50 %
50 %
22 hours @ 125°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flash Point >= 200 °C
>= 392 °F