Material Notes:
PRESEAL TPE 6071 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasketing and grounding applications. Conductivity is achieved with a silver coated glass sphere and fiber combination. PRESEAL TPE 6071 can be extruded like an ordinary thermoplastic elastomer thus giving great new possibilities in mass production. It has adhesion to selected thermoplastics, which opens construction possibilities with co-extrusion e.g. in making combined weather/dust/EMI gaskets. Recyclability is an added value. The material is silicone free. Typical applications include EMI gaskets in mobile phones, mobile phone * Tension test bar according to ISO 527 base stations and other wireless communication environment as well as in military applications.Information provided by Premix Thermoplastics Inc.
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
ISO 7619
Tensile Strength, Ultimate 0.700 MPa
102 psi
ISO 37*
Tensile Strength, Yield 0.700 MPa
102 psi
ISO 37*
Elongation at Break 290 %
290 %
ISO 37*
Elongation at Yield 150 %
150 %
ISO 37*
Modulus of Elasticity 0.00400 GPa
0.580 ksi
ISO 178
Compressive Modulus 0.0480 GPa
6.96 ksi
At 10% Compression; ISO 7743
0.0500 GPa
7.25 ksi
At 15% Compression; ISO 7743
0.0520 GPa
7.54 ksi
At 18% Compression; ISO 7743
Tear Strength 6.40 kN/m
36.5 pli
ISO 34-C
Compression Set 50 %
50 %
At 85°C, 24 hours; ISO 815:1991
Electrical Properties Metric English Comments
Volume Resistivity <= 0.0030 ohm-cm
<= 0.0030 ohm-cm
ISO Mil-G-835388
Shielding Effectiveness 100 dB
100 dB
ISO ARP1705, 20-700 MHz
Processing Properties Metric English Comments
Middle Barrel Temperature 180 °C
356 °F
Zone 2; Cylinder
180 °C
356 °F
Zone 1; Cylinder
190 °C
374 °F
Zone 3; Cylinder
190 °C
374 °F
Zone 4; Cylinder
200 °C
392 °F
Zone 5; Cylinder
200 °C
392 °F
Zone 6; Cylinder
Die Temperature 200 °C
392 °F
Zones 1-5
Drying Temperature 60.0 °C

@Time 10800 sec
140 °F

@Time 3.00 hour
Pre-drying; If stored for longer than 1 year
Moisture Content <= 0.040 %
<= 0.040 %
When Produced
Shelf Life 12.0 Month
12.0 Month
Normal Storing Conditions
Descriptive Properties Value Comments
Appearance Granule
Color Grey
Users viewing this material also viewed the following: