Material Notes:
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
(Dry)
Water Absorption 3.2 %
3.2 %
initially dry
Moisture Absorption at Equilibrium 0.90 %
0.90 %
initially dry
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
Elongation at Break 1.7 %
1.7 %
Tensile Modulus 11.4 GPa
1650 ksi
Charpy Impact Unnotched 3.50 J/cm²

@Temperature -30.0 °C
16.7 ft-lb/in²

@Temperature -22.0 °F
5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
1.30 J/cm²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
(Dry)
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
Vicat Softening Point 205 °C

@Load 5.10 kg
401 °F

@Load 11.2 lb
50°C/h
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 350 V
350 V